繰返し重ね接合圧延と時効付き低温圧延との両方の組み合わせによるCu-2.0mass%Ni-0.5mass%Si-0.1mass%Zr合金の機械的性質の改善
Improvement in Mechanical Properties of a Cu-2.0 mass%Ni-0.5 mass%Si-0.1 mass%Zr Alloy by Combining Both Accumulative Roll-Bonding and Cryo-Rolling with Aging
著者 (5件):
TAKAGAWA Yusaku
(Div. of Mechanical Sci. and Engineering, Graduate School of Natural Sci. and Technol., Kanazawa Univ.)
,
TSUJIUCHI Yukinaru
(Div. of Mechanical Sci. and Engineering, Graduate School of Natural Sci. and Technol., Kanazawa Univ.)
,
WATANABE Chihiro
(Div. of Innovative Technol. and Sci., Graduate School of Natural Sci. and Technol., Kanazawa Univ.)
,
MONZEN Ryoichi
(Div. of Innovative Technol. and Sci., Graduate School of Natural Sci. and Technol., Kanazawa Univ.)
,
TSUJI Nobuhiro
(Dep. of Materials Sci. and Engineering, Kyoto Univ.)
資料名:
Materials Transactions
(Materials Transactions)
巻:
54
号:
1
ページ:
1-8 (J-STAGE)
発行年:
2013年
JST資料番号:
G0668A
ISSN:
1345-9678
資料種別:
逐次刊行物 (A)
記事区分:
原著論文
発行国:
日本 (JPN)
言語:
英語 (EN)