文献
J-GLOBAL ID:201602252864153647
整理番号:16A0716253
Bi0.487Na0.427K0.06Ba0.026TiO3-xCeO2反強誘電性セラミックの強化されたエネルギー貯蔵と誘電特性
Enhanced energy storage and dielectric properties of Bi0.487Na0.427K0.06Ba0.026TiO3-xCeO2 anti-ferroelectric ceramics
著者 (5件):
Liu Guocai
(State Key Laboratory of Solidification Processing, School of Materials Science and Engineering, Northwestern Polytechnical University, Xi’an 710072, China)
,
Fan Huiqing
(State Key Laboratory of Solidification Processing, School of Materials Science and Engineering, Northwestern Polytechnical University, Xi’an 710072, China)
,
Dong Guangzhi
(State Key Laboratory of Solidification Processing, School of Materials Science and Engineering, Northwestern Polytechnical University, Xi’an 710072, China)
,
Shi Jing
(State Key Laboratory of Solidification Processing, School of Materials Science and Engineering, Northwestern Polytechnical University, Xi’an 710072, China)
,
Chang Qi
(State Key Laboratory of Solidification Processing, School of Materials Science and Engineering, Northwestern Polytechnical University, Xi’an 710072, China)
資料名:
Journal of Alloys and Compounds
(Journal of Alloys and Compounds)
巻:
664
ページ:
632-638
発行年:
2016年04月15日
JST資料番号:
D0083A
ISSN:
0925-8388
資料種別:
逐次刊行物 (A)
記事区分:
原著論文
発行国:
オランダ (NLD)
言語:
英語 (EN)