Ni中間層がある場合とない場合のクラッド鋼管の界面の破壊靭性と水素脆化感受性【Powered by NICT】
Fracture toughness and hydrogen embrittlement susceptibility on the interface of clad steel pipes with and without a Ni-interlayer
著者 (6件):
Jemblie L.
(Department of Engineering Design and Materials, NTNU, 7456 Trondheim, Norway)
,
Bjaaland H.
(Department of Engineering Design and Materials, NTNU, 7456 Trondheim, Norway)
,
Nyhus B.
(SINTEF Materials and Chemistry, 7456 Trondheim, Norway)
,
Olden V.
(SINTEF Materials and Chemistry, 7456 Trondheim, Norway)
,
Akselsen O.M.
(Department of Engineering Design and Materials, NTNU, 7456 Trondheim, Norway)
,
Akselsen O.M.
(SINTEF Materials and Chemistry, 7456 Trondheim, Norway)
資料名:
Materials Science & Engineering. A. Structural Materials: Properties, Microstructure and Processing
(Materials Science & Engineering. A. Structural Materials: Properties, Microstructure and Processing)
巻:
685
ページ:
87-94
発行年:
2017年
JST資料番号:
D0589B
ISSN:
0921-5093
資料種別:
逐次刊行物 (A)
記事区分:
原著論文
発行国:
オランダ (NLD)
言語:
英語 (EN)