500°Cでの超臨界水への長期曝露後の合金310Sステンレス鋼の内部酸化と割れ感受性【Powered by NICT】
Internal oxidation and crack susceptibility of alloy 310S stainless steel after long term exposure to supercritical water at 500°C
著者 (12件):
Behnamian Yashar
(Department of Chemical and Materials Engineering, University of Alberta, Edmonton, Alberta T6G 1H9, Canada)
,
Mostafaei Amir
(Department of Mechanical Engineering and Materials Science, University of Pittsburgh, Pittsburgh, PA 15261, USA)
,
Kohandehghan Alireza
(Department of Chemical and Materials Engineering, University of Alberta, Edmonton, Alberta T6G 1H9, Canada)
,
Amirkhiz Babak Shalchi
(Canmet MATERIALS, Natural Resources Canada, Hamilton, ON L8P 0A5, Canada)
,
Li Jian
(Canmet MATERIALS, Natural Resources Canada, Hamilton, ON L8P 0A5, Canada)
,
Zahiri Ramin
(Department of Chemical and Materials Engineering, University of Alberta, Edmonton, Alberta T6G 1H9, Canada)
,
Aghaie Ermia
(Department of Chemical and Materials Engineering, University of Alberta, Edmonton, Alberta T6G 1H9, Canada)
,
Zheng Wenyue
(Canmet MATERIALS, Natural Resources Canada, Hamilton, ON L8P 0A5, Canada)
,
Guzonas David
(Canadian Nuclear Laboratories, Chalk River Laboratories, Chalk River, ON K0J 1J0, Canada)
,
Chmielus Markus
(Department of Mechanical Engineering and Materials Science, University of Pittsburgh, Pittsburgh, PA 15261, USA)
,
Chen Weixing
(Department of Chemical and Materials Engineering, University of Alberta, Edmonton, Alberta T6G 1H9, Canada)
,
Luo Jing Li
(Department of Chemical and Materials Engineering, University of Alberta, Edmonton, Alberta T6G 1H9, Canada)
資料名:
Journal of Supercritical Fluids
(Journal of Supercritical Fluids)
巻:
120
号:
P1
ページ:
161-172
発行年:
2017年
JST資料番号:
W1591A
ISSN:
0896-8446
資料種別:
逐次刊行物 (A)
記事区分:
原著論文
発行国:
オランダ (NLD)
言語:
英語 (EN)