文献
J-GLOBAL ID:201702257856677537
整理番号:17A0446104
窒化けい素活性金属ろう付け基板における銅層のセラミックと剥離における亀裂形成に及ぼす高温度サイクルの影響【Powered by NICT】
Effect of high temperature cycling on both crack formation in ceramics and delamination of copper layers in silicon nitride active metal brazing substrates
著者 (7件):
Miyazakia Hiroyuki
(National Institute of Advanced Industrial Science and Technology (AIST), Nagoya 463-8560, Japan)
,
Iwakiri Shoji
(Ceramic Research Dept., Denka Co., Ltd. Omuta-shi, Fukuoka prefecture 836-8510, Japan)
,
Hirao Kiyoshi
(National Institute of Advanced Industrial Science and Technology (AIST), Nagoya 463-8560, Japan)
,
Fukuda Shinji
(National Institute of Advanced Industrial Science and Technology (AIST), Nagoya 463-8560, Japan)
,
Izu Noriya
(National Institute of Advanced Industrial Science and Technology (AIST), Nagoya 463-8560, Japan)
,
Yoshizawa Yu-ichi
(National Institute of Advanced Industrial Science and Technology (AIST), Nagoya 463-8560, Japan)
,
Hyuga Hideki
(National Institute of Advanced Industrial Science and Technology (AIST), Nagoya 463-8560, Japan)
資料名:
Ceramics International
(Ceramics International)
巻:
43
号:
6
ページ:
5080-5088
発行年:
2017年
JST資料番号:
H0705A
ISSN:
0272-8842
資料種別:
逐次刊行物 (A)
記事区分:
原著論文
発行国:
イギリス (GBR)
言語:
英語 (EN)