8mo1%イットリア安定化ジルコニアの焼結性に及ぼす酸化マンガンの影響【Powered by NICT】
Effect of manganese oxide on the sinterability of 8mol% yttria-stabilized zirconia
著者 (9件):
Chong F.D.
(Department of Mechanical Engineering, Faculty of Engineering, University of Malaya, 50603 Kuala Lumpur, Malaysia)
,
Tan C.Y.
(Department of Mechanical Engineering, Faculty of Engineering, University of Malaya, 50603 Kuala Lumpur, Malaysia)
,
Singh R.
(Department of Mechanical Engineering, Faculty of Engineering, University of Malaya, 50603 Kuala Lumpur, Malaysia)
,
Muchtar A.
(Fuel Cell Institute, Universiti Kebangsaan Malaysia, 43600, Selangor, Malaysia)
,
Somalu M.R.
(Fuel Cell Institute, Universiti Kebangsaan Malaysia, 43600, Selangor, Malaysia)
,
Ng C.K.
(Department of Mechanical Engineering, Faculty of Engineering, University of Malaya, 50603 Kuala Lumpur, Malaysia)
,
Yap B.K.
(Department of Electronics and Communication, College of Engineering, Universiti Tenaga Nasional, 43000, Selangor, Malaysia)
,
Teh Y.C.
(Department of Mechanical Engineering, Faculty of Engineering, University of Malaya, 50603 Kuala Lumpur, Malaysia)
,
Tan Y.M.
(Department of Mechanical Engineering, Faculty of Engineering, University of Malaya, 50603 Kuala Lumpur, Malaysia)
資料名:
Materials Characterization
(Materials Characterization)
巻:
120
ページ:
331-336
発行年:
2016年
JST資料番号:
D0448C
ISSN:
1044-5803
資料種別:
逐次刊行物 (A)
記事区分:
原著論文
発行国:
アメリカ合衆国 (USA)
言語:
英語 (EN)