Na_2SO_4+V_2O_5溶融塩に曝露されたGd_2O_3 Yb_2O_3共ドープY_2O_3安定化ZrO_2熱障壁酸化物の高温腐食評価【Powered by NICT】
Hot corrosion evaluation of Gd2O3-Yb2O3 co-doped Y2O3 stabilized ZrO2 thermal barrier oxides exposed to Na2SO4+V2O5 molten salt
著者 (12件):
Guo Lei
(School of Materials Science and Engineering, Tianjin University, No. 92, Weijin Road, Tianjin 300072, China)
,
Guo Lei
(Tianjin Key Laboratory of Advanced Joining Technology, Tianjin University, No. 92, Weijin Road, Tianjin 300072, China)
,
Guo Lei
(Key Lab of Advanced Ceramics and Machining Technology of Ministry of Education, Tianjin University, No. 92, Weijin Road, Tianjin 300072, China)
,
Zhang Chenglong
(School of Materials Science and Engineering, Tianjin University, No. 92, Weijin Road, Tianjin 300072, China)
,
Zhang Chenglong
(Tianjin Key Laboratory of Advanced Joining Technology, Tianjin University, No. 92, Weijin Road, Tianjin 300072, China)
,
Li Mingzhu
(School of Materials Science and Engineering, Tianjin University, No. 92, Weijin Road, Tianjin 300072, China)
,
Li Mingzhu
(Tianjin Key Laboratory of Advanced Joining Technology, Tianjin University, No. 92, Weijin Road, Tianjin 300072, China)
,
Sun Wei
(School of Materials Science and Engineering, Tianjin University, No. 92, Weijin Road, Tianjin 300072, China)
,
Zhang Zhaoyang
(School of Materials Science and Engineering, Tianjin University, No. 92, Weijin Road, Tianjin 300072, China)
,
Ye Fuxing
(School of Materials Science and Engineering, Tianjin University, No. 92, Weijin Road, Tianjin 300072, China)
,
Ye Fuxing
(Tianjin Key Laboratory of Advanced Joining Technology, Tianjin University, No. 92, Weijin Road, Tianjin 300072, China)
,
Ye Fuxing
(Key Lab of Advanced Ceramics and Machining Technology of Ministry of Education, Tianjin University, No. 92, Weijin Road, Tianjin 300072, China)
資料名:
Ceramics International
(Ceramics International)
巻:
43
号:
2
ページ:
2780-2785
発行年:
2017年
JST資料番号:
H0705A
ISSN:
0272-8842
資料種別:
逐次刊行物 (A)
記事区分:
原著論文
発行国:
イギリス (GBR)
言語:
英語 (EN)