Ti_1(VFe)CrNi_0 2+xwt%LaNi_5(x=0, 2.5, 4, 5, 6, 10, 20)金属水素化物合金の電気化学的活性化特性に及ぼす微細構造と相組成の影響【Powered by NICT】
Effects of microstructure and phase composition on the electrochemical activation properties of Ti1.8(VFe)CrNi0.2 + xwt.%LaNi5(x=0, 2.5, 4, 5, 6, 10, 20) metal hydride alloys
著者 (5件):
Cui Junjie
(School of Material Science and Engineering, Inner Mongolia University of Technology, Hohhot 010051, China)
,
Cui Junjie
(Information and Network Center, Inner Mongolia University of Science and Technology, Baotou 010014, China)
,
Liu Xiangdong
(School of Material Science and Engineering, Inner Mongolia University of Technology, Hohhot 010051, China)
,
Lue Kai
(School of Material Science and Engineering, Inner Mongolia University of Technology, Hohhot 010051, China)
,
Shang Junxiao
(School of Material Science and Engineering, Inner Mongolia University of Technology, Hohhot 010051, China)
資料名:
International Journal of Hydrogen Energy
(International Journal of Hydrogen Energy)
巻:
43
号:
2
ページ:
580-591
発行年:
2018年
JST資料番号:
B0192B
ISSN:
0360-3199
資料種別:
逐次刊行物 (A)
記事区分:
原著論文
発行国:
イギリス (GBR)
言語:
英語 (EN)