J-GLOBAL ID:201802276305558800
整理番号:18A1723384
SiC繊維強化材における熱分解炭素被覆の適切な厚さによるナイトSiC/SiC複合材料の安全な準延性の確保【JST・京大機械翻訳】
Appropriate thickness of pyrolytic carbon coating on SiC fiber reinforcement to secure reasonable quasi-ductility on NITE SiC/SiC composites
著者 (4件):
Nakazato Naofumi
(College of Design and Manufacturing Technology, Muroran Institute of Technology, Muroran, Hokkaido, Japan)
,
Kishimoto Hirotatsu
(College of Design and Manufacturing Technology, Muroran Institute of Technology, Muroran, Hokkaido, Japan)
,
Kishimoto Hirotatsu
(Organization of Advanced Sustainability Initiative for Energy System/Material (OASIS), Muroran Institute of Technology, Muroran, Hokkaido, Japan)
,
Park Joon-Soo
(Organization of Advanced Sustainability Initiative for Energy System/Material (OASIS), Muroran Institute of Technology, Muroran, Hokkaido, Japan)
資料名:
Ceramics International
(Ceramics International)
巻:
44
号:
16
ページ:
19307-19313
発行年:
2018年
JST資料番号:
H0705A
ISSN:
0272-8842
資料種別:
逐次刊行物 (A)
記事区分:
原著論文
発行国:
イギリス (GBR)
言語:
英語 (EN)