文献
J-GLOBAL ID:202002220915711909
整理番号:20A0790301
1250°CにおけるCMASにより攻撃されたm-YTaO_4の熱障壁材料の腐食挙動【JST・京大機械翻訳】
The corrosion behaviors of thermal barrier material of M-YTaO4 attacked by CMAS at 1250 °C
著者 (4件):
Yang Wenqi
(School of Materials Science and Engineering, Tianjin University, Tianjin Key Laboratory of Advanced Joining Technology, Key Lab of Advanced Ceramics and Machining Technology of Ministry of Education, No. 92, Weijin Road, Tianjin, 300072, China)
,
Ye Fuxing
(School of Materials Science and Engineering, Tianjin University, Tianjin Key Laboratory of Advanced Joining Technology, Key Lab of Advanced Ceramics and Machining Technology of Ministry of Education, No. 92, Weijin Road, Tianjin, 300072, China)
,
Yan Shuai
(School of Materials Science and Engineering, Tianjin University, Tianjin Key Laboratory of Advanced Joining Technology, Key Lab of Advanced Ceramics and Machining Technology of Ministry of Education, No. 92, Weijin Road, Tianjin, 300072, China)
,
Guo Lei
(School of Materials Science and Engineering, Tianjin University, Tianjin Key Laboratory of Advanced Joining Technology, Key Lab of Advanced Ceramics and Machining Technology of Ministry of Education, No. 92, Weijin Road, Tianjin, 300072, China)
資料名:
Ceramics International
(Ceramics International)
巻:
46
号:
7
ページ:
9311-9318
発行年:
2020年
JST資料番号:
H0705A
ISSN:
0272-8842
資料種別:
逐次刊行物 (A)
記事区分:
原著論文
発行国:
イギリス (GBR)
言語:
英語 (EN)