Mn-Si-Cr鋼におけるナノサイズ残留オーステナイトの平面欠陥の研究【JST・京大機械翻訳】
The study of the planar defects of the nano-sized retained austenite in Mn-Si-Cr steel
著者 (5件):
Qiu Jiajia
(School of Mechanical, Electronic and Control Engineering, Materials Science and Engineering Research Center, Beijing Jiaotong University, Beijing 100044, China)
,
Zhang Min
(School of Mechanical, Electronic and Control Engineering, Materials Science and Engineering Research Center, Beijing Jiaotong University, Beijing 100044, China)
,
Liu Xinyang
(School of Mechanical, Electronic and Control Engineering, Materials Science and Engineering Research Center, Beijing Jiaotong University, Beijing 100044, China)
,
Zhang Xinxin
(School of Mechanical, Electronic and Control Engineering, Materials Science and Engineering Research Center, Beijing Jiaotong University, Beijing 100044, China)
,
Tan Zhunli
(School of Mechanical, Electronic and Control Engineering, Materials Science and Engineering Research Center, Beijing Jiaotong University, Beijing 100044, China)
資料名:
Materials Letters
(Materials Letters)
巻:
266
ページ:
Null
発行年:
2020年
JST資料番号:
E0935A
ISSN:
0167-577X
資料種別:
逐次刊行物 (A)
記事区分:
短報
発行国:
オランダ (NLD)
言語:
英語 (EN)