文献
J-GLOBAL ID:202002268430205404
整理番号:20A0230025
リチウム及び黒鉛負極を用いたLiNi_0.5Mn_0.3Co_0.2O_2表面膜形成に及ぼす電解質添加物の影響【JST・京大機械翻訳】
Effect of Electrolyte Additives on the LiNi0.5Mn0.3Co0.2O2 Surface Film Formation with Lithium and Graphite Negative Electrodes
著者 (12件):
Hekmatfar Maral
(Helmholtz Institute Ulm (HIU), Helmholtzstrasse 11, 89081, Ulm, Germany)
,
Hekmatfar Maral
(Karlsruhe Institute of Technology (KIT), P.O. Box 3640, 76021, Karlsruhe, Germany)
,
Hasa Ivana
(Helmholtz Institute Ulm (HIU), Helmholtzstrasse 11, 89081, Ulm, Germany)
,
Hasa Ivana
(Karlsruhe Institute of Technology (KIT), P.O. Box 3640, 76021, Karlsruhe, Germany)
,
Eghbal Ramtin
(Helmholtz Institute Ulm (HIU), Helmholtzstrasse 11, 89081, Ulm, Germany)
,
Eghbal Ramtin
(Karlsruhe Institute of Technology (KIT), P.O. Box 3640, 76021, Karlsruhe, Germany)
,
Carvalho Diogo V.
(Helmholtz Institute Ulm (HIU), Helmholtzstrasse 11, 89081, Ulm, Germany)
,
Carvalho Diogo V.
(Karlsruhe Institute of Technology (KIT), P.O. Box 3640, 76021, Karlsruhe, Germany)
,
Moretti Arianna
(Helmholtz Institute Ulm (HIU), Helmholtzstrasse 11, 89081, Ulm, Germany)
,
Moretti Arianna
(Karlsruhe Institute of Technology (KIT), P.O. Box 3640, 76021, Karlsruhe, Germany)
,
Passerini Stefano
(Helmholtz Institute Ulm (HIU), Helmholtzstrasse 11, 89081, Ulm, Germany)
,
Passerini Stefano
(Karlsruhe Institute of Technology (KIT), P.O. Box 3640, 76021, Karlsruhe, Germany)
資料名:
Advanced Materials Interfaces
(Advanced Materials Interfaces)
巻:
7
号:
1
ページ:
e1901500
発行年:
2020年
JST資料番号:
W2484A
ISSN:
2196-7350
資料種別:
逐次刊行物 (A)
記事区分:
原著論文
発行国:
アメリカ合衆国 (USA)
言語:
英語 (EN)