Deterioration Mechanism and Estimation of Durability of Reinforced Concrete in Marine Environment - 5-year Exposure.

海洋環境にある鉄筋コンクリートの劣化機構および耐久性評価 5年曝露
Author (1):
Material:
Issue: 13  Page: 31-38  Publication year: Feb. 28, 2001 
JST Material Number: L0250A  ISSN: 0916-2054  Document type: Article
Article type: 解説  Country of issue: Japan (JPN)  Language: ENGLISH (EN)
Thesaurus term:
Thesaurus term/Semi thesaurus term
Keywords indexed to the article.
All keywords is available on JDreamIII(charged).
On J-GLOBAL, this item will be available after more than half a year after the record posted. In addtion, medical articles require to login to MyJ-GLOBAL.
,...
   To see more with JDream III (charged).   {{ this.onShowAbsJLink("http://jdream3.com/lp/jglobal/index.html?docNo=01A0381294&from=J-GLOBAL&jstjournalNo=L0250A") }}
JST classification (1):
JST classification
Category name(code) classified by JST.
Mortar,concrete 
Terms in the title (4):
Terms in the title
Keywords automatically extracted from the title.

Return to Previous Page