Tensile properties of HIP’ed Ti-6Al-4V alloy after vacuum sintering.
真空焼結後HIP処理したTi-6Al-4V合金の引張性質
Publisher site
{{ this.onShowPLink() }}
Copy service
{{ this.onShowCLink("http://jdream3.com/copy/?sid=JGLOBAL&noSystem=1&documentNoArray=96A0806806©=1") }}
Volume:
46
Issue:
8
Page:
371-376
Publication year:
Aug. 1996
JST Material Number:
F0772A
ISSN:
0451-5994
CODEN:
KEIKA6
Document type:
Article
Article type:
原著論文
Country of issue:
Japan (JPN)
Language:
JAPANESE (JA)
Thesaurus term:
Thesaurus term/Semi thesaurus term Keywords indexed to the article. All keywords is available on JDreamIII(charged). On J-GLOBAL, this item will be available after more than half a year after the record posted. In addtion, medical articles require to login to MyJ-GLOBAL.
To see more with JDream III (charged).
{{ this.onShowAbsJLink("http://jdream3.com/lp/jglobal/index.html?docNo=96A0806806&from=J-GLOBAL&jstjournalNo=F0772A") }}
JST classification (2):
JST classification
Category name(code) classified by JST.