Four-year water degradation of total-etch adhesives bonded to dentin

象牙質に接合したトータルエッチング接着剤の4年後の水劣化状況
Author (8):
Material:
Volume: 82  Issue:Page: 136-140  Publication year: 2003 
JST Material Number: O3556A  ISSN: 0022-0345  Document type: Article
Country of issue: Other (ZZZ)  Language: ENGLISH (EN)
Reference (24):
  • ARMSTRONG, SR. Mode of failure in the dentin-adhesive resin-resin composite bonded joint as determined by strength-based (μTBS) and fracture-based (CNSB) mechanical testing. Dent Mater. 2001, 17, 201-210
  • ARMSTRONG, SR. The influence of water storage and C-factor on the dentin-resin composite microtensile bond strength and debond pathway utilizing a filled and unfilled adhesive resin. Dent Mater. 2001, 17, 268-276
  • BOGHOSIAN, A. Clinical evaluation of a filled adhesive system in Class 5 restorations. Compend Contin Educ Dent. 1996, 7, 750-752, 754-757
  • BURROW, MF. Dentin bond durability after three years using a dentin bonding agent with and without priming. Dent Mater. 1996, 12, 302-307
  • ELIADES, G. Heterogeneous distribution of single-bottle adhesive monomers in the resin-dentin interdiffusion zone. Dent Mater. 2001, 17, 277-283