Effect of SUS316L stainless steel surface conditions on the wetting of molten multi-component oxides ceramic

溶融多成分酸化物セラミックの濡れ性に対するSUS316Lステンレス鋼の表面状態の影響
Author (5):
Material:
Volume: 327  Page: 470-477  Publication year: Feb. 01, 2015 
JST Material Number: B0707B  ISSN: 0169-4332  Document type: Article
Article type: 原著論文  Country of issue: Netherlands (NLD)  Language: ENGLISH (EN)
Thesaurus term:
Thesaurus term/Semi thesaurus term
Keywords indexed to the article.
All keywords is available on JDreamIII(charged).
On J-GLOBAL, this item will be available after more than half a year after the record posted. In addtion, medical articles require to login to MyJ-GLOBAL.

Semi thesaurus term:
Thesaurus term/Semi thesaurus term
Keywords indexed to the article.
All keywords is available on JDreamIII(charged).
On J-GLOBAL, this item will be available after more than half a year after the record posted. In addtion, medical articles require to login to MyJ-GLOBAL.

JST classification (2):
JST classification
Category name(code) classified by JST.
Ceramic coating to metallic materials  ,  Solid-liquid interface 
Terms in the title (5):
Terms in the title
Keywords automatically extracted from the title.

Return to Previous Page