Effect of intermediate layer on wear-delamination life of low-frictional SiC-2.6mass%Ti film sputter-deposited on titanium substrate

チタン基板上にスパッタ蒸着した低摩擦SiC-2.6質量%Ti膜の摩耗剥離に及ぼす中間層の影響