S. Yoshida, K. Wada, T. Fujimura, A. Yamada, M. Kato, J. Matsuoka, N. Soga. Evaluation of Sinking-In and Cracking Behavior of Soda-Lime Glass under Varying Angle of Trigonal Pyramid Indenter. Frontiers in Materials. 2016. 3. 54. 1-9
S. Yoshida. Indentation deformation and cracking in oxide glass -toward understanding of crack nucleation. J. Non-Cryst. Solids:X. 2019. 1. 100009-1-100009-9
Indentation-induced transient and permanent structural changes of glass probed by Raman spectroscopy
(Annual Meeting of International Commission on Glass 2018)
In-situ evaluation of structural changes of glass under a sharp indenter
(The Sixth International Indentation Workshop 2018)
In-Situ Raman Measurements of Silicate Glasses during Indentation (Invited)
(7th International Congress on Ceramics 2018)
An indentation microscope: A powerful tool for evaluating deformation and cracking in glass (Invited)
(Special Seminar at NITech 2017)
Indentation Deformation and Fracture of Glasses (Invited)
(Society of Glass Technology Centenary Conference 2016)
2016/09/05 - Ernst Abbe Fund 14th Otto Schott Research Award
2014/06 - 日本セラミックス協会 2013 JCerSJ優秀論文賞 Heat capacity measurements of 75SiO<SUB>2</SUB>-6B<SUB>2</SUB>O<SUB>3</SUB>-10Al<SUB>2</SUB>O<SUB>3</SUB>-9MO (M=Mg, Ca, Sr and Ba) glasses and melts 75SiO<SUB>2</SUB>-6B<SUB>2</SUB>O<SUB>3</SUB>-10Al<SUB>2</SUB>O<SUB>3</SUB>-9MO (M=Mg, Ca, Sr and Ba)
2011/06 - 日本セラミックス協会 2010 JCerSJ優秀論文賞 Effect of B<SUB>2</SUB>O<SUB>3</SUB> content on crack initiation under Vickers indentation test
2009/07/01 - ICMAT & IUMRS-ICA 2009 Best Poster Award Inelastic Deformation of Glass beneath Sharp Diamond Indenters